MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Tixogel® MP 250 Modified Montmorillonite
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: TIXOGEL MP250 is a maximum performance modified montmorillonite designed to be used in aromatic and polar systems that exhibit medium to high polarity. TIXOGEL MP250 functions as a thixotropic rheology modifier generating properties such as flow control and anti-setting. TIXOGEL MP250 provides reliable and reproducible rheological properties in solvent based paints, stains, enamels, primers, and inks as well as other applications. TIXOGEL MP250 does not require the use of a polar activator to achieve full efficiency.

Application:

  • Oil based paints and stains
  • Adhesives
  • Caulks and sealants
  • Cosmetics and personal care
  • Inks

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 19.0 - 25.0 lb/ft³
Density 1.50 g/cc
Particle Mesh Size <= 200 Mesh70%
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 3.0 %
Loss on Ignition(%) 36 - 44 %
@Temperature 1000 °C
 
Descriptive Properties
Color/FormVery light cream free flowing, divided powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Tixogel® EZ Modified Montmorillonite
BYK Rheocin® T Rheological Modification
BYK Rheocin® Rheological Modification
BYK Rheocin® PC Polymer
BYK Pure Thix® 1442 Associative Thickener for Water or Water Phase for Personal Care

PBYK117 / 185114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.