MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon H5650 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Alathon H5650 is a multi-purpose high-flow resin that exhibits enhanced processing and thermal stability for fast cycling in multi-cavity stack molds. This resin also exhibits good color and organoleptic properties. Typical applications are rigid food containers and aerosol can overcaps.

Availability: North America

Application: Caps & Closures; TWIM Food Containers

Market: Consumer Products; Rigid Packaging

Processing Method: Injection Molding

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.593 - 0.625 g/ccASTM D1895
Density 0.956 g/ccASTM D1505
Melt Flow 50.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 64.0ASTM D2240
Tensile Strength at Break 24.0 MPaASTM D638
Tensile Strength, Yield 25.8 MPaASTM D638
Elongation at Break 4.80 %ASTM D638
Flexural Modulus 1145 MPa2% Secant; ASTM D790
 1352 MPa1% Secant; ASTM D790
 1586 MPaASTM D790
Izod Impact, Notched 2.75 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 130.9 °CASTM D3418
Crystallization Temperature 116.1 °CASTM D3418
Vicat Softening Point 125 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9033 / 323961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.