MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Total PPH 4026 Polypropylene Homopolymer, Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.

Polypropylene PPH 4026 is intended for applications like hot fill food packaging, labeling, twist or lamination films.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Thickness 50.0 microns
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ISO 2039-2
Film Tensile Strength at Yield, MD 31.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 29.0 MPaISO 527-3
Tensile Strength, Yield 39.0 MPaISO 527-2
Film Elongation at Break, MD 470 %ISO 527-3
Film Elongation at Break, TD 580 %ISO 527-3
Elongation at Yield 9.0 %ISO 527-2
Tensile Modulus 2050 MPaISO 527-2
Flexural Modulus 2000 MPaISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²ISO 180
Charpy Impact, Notched 6.00 kJ/m²ISO 179
Elmendorf Tear Strength, MD 0.600 g/micronISO 6383-2
Elmendorf Tear Strength, TD 9.00 g/micronISO 6383-2
Dart Drop Test 80.0 gISO 7765-1
Film Tensile Strength at Break, MD 62.0 MPaISO 527-3
Film Tensile Strength at Break, TD 35.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 110 °C120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C120°C per hour; ISO 752
Vicat Softening Point 97.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 153 °C
@Load 1.02 kg
50°C per hour; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 14 %ISO 14782
Gloss 51 %at 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 4030 Polypropylene Homopolymer
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming
Total PPH 4070 Polypropylene Homopolymer
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications

PTOTAL791 / 130516

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.