MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Pulpsil® 960 S Silicone Surfactant
Categories: Fluid

Material Notes: PULPSIL® 960 S is a water dispersible, hydrolytically stable silicone surfactant based on a polyether modified silicone fluid.

Application: PULPSIL® 960 S was developed for application in pulp and paper industry. PULPSIL® 960 S:

  • enhances the efficacy of paper deaerators at a dosage of 1.0 - 10.0 % referred to solid material of deaerator.
  • improves the drainage / deaerating in the pulp process at following dosage levels:
  • hardwood: 0.02 - 0.10 % referred to fibers
  • softwood: 0.2 - 1.0 % referred to fibers
  • works itself as a booster for pulp-defoamers above its cloud point at a dosage of 2.0 - 20 % referred to active material of defoamer.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
@Pressure 0.1013 MPa
Kinematic Viscosity 1300 cSt
 
Thermal PropertiesOriginal ValueComments
Flash Point 120 °CISO 2719
Ignition Temperature 364 °CEN 14522
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.448DIN 51423
 
Descriptive Properties
Appearanceslightly brownish fluid
Cloud point22°C1% in water, DIN EN 1890; Method A
 29°C17-25% aqueous solution of diethylene glycol monobutyl ether, DIN EN 1890; Method E
Solubility10% in ethanolsoluble
 10% in isopropyl myristatesoluble
 10% in paraffinum subliquiddumin soluble
 10% in waterdispersible

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9410 / 204939

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.