Zeptol 1020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures. Same as Zetpol 1010, except for lower saturation level allowing for sulfur cuing. FDA approved. |