Hifax TYC 2097X black is a 15% mineral filled high impact polypropylene copolymer for injection molding. It combines an excellent flowability with very good stiffness/ impact properties. The grade has been specifically designed for molding of large exterior parts that requires good dimensional stability. Availability: Europe Application: Bumpers Market: Automotive Processing Method: Injection Molding Attribute: Good Impact Resistance; High Flow; Paintable Information provided by LyondellBasell. |