MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin PTFE D-210 DISPERSION Polytetrafluoroethylene Aqueous Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Daikin PTFE D-210 is a homopolymer polytetrafluoroethylene aqueous dispersion manufactured without the use of PFOA. D-210 has been designed for general purpose use in yarn coating, packing impregnation, glass fabric coating and release coating formulation applications. D-210 contains a more environmentally friendly surfactant that leaves fewer residues in the substrate than traditional surfactants.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 - 1.53 g/cc
Solids Content 59 - 61 %
pH 8.5 - 10.5
Viscosity <= 35 cP
@Temperature 25.0 °C
Thickness <= 14.0 micronsCritical Cracking Thickness
 
Descriptive Properties
AppearanceMilky White Liquid
Surfactant Content6-7.2%PTFE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shandong Dongyue Polymer DF-302 PTFE Aqueous Dispersion 60%
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
AGC Fluon® AD639 PTFE Aqueous Dispersion
Daikin PTFE D-310 Polytetrafluoroethylene Aqueous Dispersion
Daikin POLYFLON D-1E PTFE Dispersion

PDAIJ9894 / 209965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.