MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials GE Silicones SWS Single-component, neutral cure silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: SWS weatherproofing sealant is a single-component, neutral cure silicone, which is an excellent candidate for use in new or remedial weathersealing applications. SWS exhibits negligible change in physical properties after weathering and upon cure, becomes a low-modulus, formed-in-place durable rubber building joint & glazing sealant.

Features: Silicone Durability, High Performance, ±50% Movement Capacity, Primerless Adhesion. SWS is an excellent candidate to consider: As a weatherproofing material when sealing between dissimilar or similar materials in either new or remedial glazing and sealing applications, window perimeters and punched openings. For sealing to precast concrete, site cast concrete and tilt-up concrete joints. As a general purpose sealant for seams and curtainwall frames, screw heads, back pans, etc. SWS is not: For use in structural glazing applications. For use in food contact applications. For use in applications where the product will be in continuous contact with water. Paintable (except when using SilShield* 2400 or Optic* 2401 silicone elastomeric coating). For use on wet, damp, frozen or contaminated surfaces.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2222ASTM D2240
Tensile Stress at Strain  0.130 MPa
@Strain 25 %
18.9 psi
@Strain 25 %
ASTM C1135
 0.210 MPa
@Strain 50 %
30.5 psi
@Strain 50 %
ASTM C1135
Peel Strength >= 7.89 kN/m>= 45.0 pliASTM C794
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -48.3 °C-55.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 50.0 °C40.0 - 122 °FApplication Temperature
Cure Time 2880 - 4320 min48.0 - 72.0 hour
 10100 - 14400 min168 - 240 hourFully Cured. Most common bead sizes.
 
Descriptive Properties
ColorAluminumSWS09
 BeigeSWS13
 BlackSWS03
 BronzeSWS97
 ChampagneSWS46
 CharcoalSWS18
 Dolphin GreySWS14
 Light GraySWS08
 LimestoneSWS04
 Monument StoneSWS21
 Precast WhiteSWS20
 Redwood TanSWS19
 SandalwoodSWS17
 Slate GreySWS16
 Special GreySWS12
 Stone GreySWS15
 WhiteSWS02
Cyclic Movement Capacity±50%ASTM C719

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9930 / 265741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.