MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huber SB 332 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: SB-332 ground ATH that provides low cost flame retardance and smoke suppression, and arc-track resistance. The medium-fine particle distribution yields desirable flow properties, good physical properties and suspension characteristics required in SMC/BMC compression molding and many rubber compounds. Applications utilizing SB-332 includes SMC/BMC electrical switch gear, appliance electrical sheet and office equipment housings along with epoxies, polishes, adhesives and coatings. A complete range of surface modifications is available to aid processing and enhance physical properties. These include silanes, stearates and wetting agents. Technical service is available.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.42 g/cc2.42 g/cc
Bulk Density 0.700 g/cc0.0253 lb/in³loose
 1.25 g/cc0.0452 lb/in³packed
Brightness 44 %44 %TAPPI
Oil Absorption >= 29 %>= 29 %29 ml/100gm
Moisture Absorption 0.250 %
@Temperature 105 °C
0.250 %
@Temperature 221 °F
Free
Particle Size <= 10 µm<= 10 µm53 percent
 11 µm11 µmMedian Particle Diameter
Particle Mesh Size 325 Mesh325 Mesh0.1% on
 325 Mesh325 Mesh99.9% through
Specific Surface Area 1.8 m²/g1.8 m²/gBET
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.0060 %0.0060 %
Loss on Ignition(%) 34.6 %
@Temperature 1000 °C
34.6 %
@Temperature 1830 °F
Na2O 0.080 %0.080 %soluble
 0.24 %0.24 %total
SiO2 0.0050 %0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalitySmoke Suppression
Market/Application: ThermosetsSMC/BMC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER766 / 300872

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.