MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANMELTTHANE® PES-537-AE Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANMELTTHANE_ PES-537-AE is a linear, saturated, high molecular polyester which is solvated in approx. 37% in organic solvents. These partially crystalline polyester type is used as basic raw material by the production of coil coating- lacquers, for lamination adhesives for the lamination of films. It is also needed for the processing of synthetic lacquers.

Application: DANMELTTHANE_ PES-537-AE is applied by the production of coil coatings-, lacquers- and plastic coatings. An additional field is the appliance as lamination adhesive by the lamination of films and foils. DANMELTTHANE_ PES-537-AE is used for textile lamination and impart for adhesives. Further, release lacquer coatings , high elastic CC-primer and gravure printing lacquers are being produced with DANMELTTHANE_ PES-537-AE.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³DIN 53.479
Solids Content 36 - 38 %36 - 38 %ASTM D 4209-82
 
Chemical PropertiesMetricEnglishComments
Acid Value 2.02.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 - 90.0 °C185 - 194 °Fsolid film, KOFLER
Glass Transition Temp, Tg 4.00 °C39.2 °FDSC-Cooling
 5.50 °C41.9 °FDSC-Heating
Flash Point -3.00 °C26.6 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.0<= 3.0DIN 6.162
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.15 %<= 0.15 %
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspecttransparent to light yellow liquid
Hydroxyl value2 mg KOH/g
Stock point5 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ120 / 294540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.