MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Indium Corp. 99.99% InBr3 Indium Tribromide, Anhydrous
Categories: Ceramic; Halide

Material Notes:
  • Boiling Point: Sublimes
  • Crystalline Form: Carmine red or yellow crystals
  • Isomorphous with: AlCl3, YCl3
  • Coordination Number: 6

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.74 g/cc4.74 g/cc
Solubility in Water 84.64 %
@Temperature 22.0 °C
84.64 %
@Temperature 71.6 °F
Molecular Weight 354.53 g/mol354.53 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 436 °C817 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00010 - 0.0010 %0.00010 - 0.0010 %
Cadmium, Cd 0.00050 - 0.0010 %0.00050 - 0.0010 %
Copper, Cu 0.00010 - 0.00020 %0.00010 - 0.00020 %
Indium, In 32.4 %32.4 %
Iron, Fe 0.00010 - 0.00020 %0.00010 - 0.00020 %
Lead, Pb 0.0010 - 0.0030 %0.0010 - 0.0030 %
Magnesium, Mg 0.00010 - 0.0010 %0.00010 - 0.0010 %
Nickel, Ni 0.0010 - 0.0020 %0.0010 - 0.0020 %
Silicon, Si 0.00010 - 0.0010 %0.00010 - 0.0010 %
Thallium, Tl 0.0010 - 0.0020 %0.0010 - 0.0020 %
Tin, Sn 0.0010 - 0.0020 %0.0010 - 0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NNIN941 / 131580

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.