MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Marco Polo MARPOL HDM 540 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: MARPOL® HDM 540 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing, and thermal stability with good color and organoleptic properties.

Recommended Applications: Rigid food containers such as 4-, 5- and 6- quart ice cream containers that are produced in fast cycling multi-cavity stack molds.

This resin complies with FDA regulation 21 CFR 177.1520 (c) 3.1a, and may be used as articles or components of articles intended for packaging or holding food, except during cooking.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.593 - 0.625 g/cc0.0214 - 0.0226 lb/in³ASTM D1895
Density 0.948 g/cc0.0342 lb/in³ASTM D1505
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength at Break 21.8 MPa3160 psi50 mm/min, Type IV; ASTM D638
Elongation at Break 5.4 %5.4 %50 mm/min, Type IV; ASTM D638
Flexural Modulus, 1% Secant 985.3 MPa142900 psi12.5 mm/min; ASTM D790B
Izod Impact, Notched 0.230 J/cm0.430 ft-lb/inASTM D256
Izod Impact, Unnotched 3.63 J/cm
@Temperature -18.0 °C
6.80 ft-lb/in
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C261 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 63.9 °C147 °FASTM D648
Vicat Softening Point 121 °C250 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO193 / 283790

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.