MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ecomass® 1002ZD96 Tungsten Filled COPA
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.
  • High Specific Gravity
  • Tungsten Powder Filled Co-Polyamide (COPA)
  • Excellent Toughness

Information provided by Technical Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 10.0 g/cc10.0 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 9.00 MPa1310 psiISO 527
Elongation at Break 500 %500 %ISO 527
Flexural Modulus 0.200 GPa29.0 ksiISO 178
Izod Impact, Notched NBNBISO 180-A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
Drying Temperature 70.0 °C158 °F
Dry Time 2 - 4 hour2 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ecomass® 1002ZC85 Stainless Steel Filled COPA
Ecomass® 720ZD88 Tungsten Filled ABS
RTP Company RTP 199 X 108940 B Polypropylene (PP), High Gravity Compound
RTP Company RTP 199 X 108940 C Polypropylene (PP), High Gravity Compound
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate

PECOM25 / 35435

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.