MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake TRUCOAT® EC4042 Extrusion Coating LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: TRUCOAT® EC4042 is a low density polyethylene resin designed for extrusion coating applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. This product also provides good heat seals at high packaging or sealing rates.

Where required, test specimens are compression molded according to ASTM D 1928 at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D4883
Melt Index of Compound 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 10.3 MPa1500 psi500 mm/min (20 in/min); ASTM D638 Type IV Specimen
Elongation at Break 400 %400 %500 mm/min (20 in/min); ASTMD 638 Type IV Specimen
Flexural Modulus, 1% Secant 193 MPa28000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 105.2 °C221.4 °FDSC Peak; ASTM D3418
Vicat Softening Point 85.0 °C185 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 329 °C<= 625 °FExtrusion coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8734 / 287844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.