Weight per Epoxide (EEW, g/eq) 217 to 244. Max color is <=6. Comments/Applications: Epoxy cresol novolac with a functionality of 5.4; highest melting ECN. Also useful in powder coatings, I.e. silicone-based formulations. Data provided by Ciba Specialty Chemicals. Ciba Specialty Chemicals has been acquired by Huntsman. |