Description: TIPELIN FB 472-02 is a film grade of high density polyethylene copolymer (with hexen-1 as comonomer) grade. The product has high molecular mass, very good Tear strength and Dart drop resistance, low gel content, good vapor barrier properties. The grade contains antioxidants and acid scavenger. Applications: TIPELIN FB 472-02 is recommended for films, bags, shopping bags, garbage bags and blend component for LDPE in shrink films. Recommended film thickness is 0.015 to 0.06 mm. (1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements on film (MD = machine direction, TD = trans direction) thickness of 0.025 mm, blow up ratio 4:1. Information provided by Molgroup Chemicals |