Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. This material complies with RoHS requirements. Standard complying - EN 50264 EI110; EN 50363-0 G10; EN50363-5 EI5 and EI8; EN50363-6 EM10; IEC 60092/360 HF90; Cenelec HD 624.6; VDE 0266 HXI1 and HXM1; VDE 0250 HI3; VDE 0207 HJ1 and HM1. Crosslinkable; Flame Retardant; Halogen Free; Low Smoke Emission; Low Toxicity; Self Extinguishing Uses: Cable Jacketing; Low Voltage Insulation; Wire & Cable Applications Availability: Asia Pacific; Europe; North America Information provided by Solvay Specialty Polymers. |