MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Inov Chem Donpanel 422 HCFC-141b Base blend polyols for PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPanel 422/ PUR blend polyols is a compound which consists of polyether polyols, surfactants, catalysts, HCFC-141B and flame retardant in a special ratio. The foam has good thermal insulation property, light in weight, high compression strength and flame retardant and other advantages. It is widely used to produce continuous sandwich panels, corrugated panels etc, which applies to make cold stores, cabinets, portable shelters and so on.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 - 1.16 g/cc1.12 - 1.16 g/cc
Density 0.0280 - 0.0350 g/cc0.00101 - 0.00126 lb/in³Free density, Manual Mix
 0.0330 - 0.0350 g/cc0.00119 - 0.00126 lb/in³Free density, High temperature machine
 >= 0.0400 g/cc>= 0.00145 lb/in³Mold density; ASTM D 1622-08
Viscosity 300 - 400 cP300 - 400 cPDynamic
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 0.140 MPa>= 20.3 psiGB/T 8813
Adhesive Bond Strength >= 0.120 MPa>= 17.4 psiGB/T 16777
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 15.0 °C
<= 0.153 BTU-in/hr-ft²-°F
@Temperature 59.0 °F
GB 3399
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 25.0 °C68.0 - 77.0 °FMaterial Temperature, Manual mix
 20.0 - 25.0 °C68.0 - 77.0 °FMaterial Temperature, High temperature machine
Mold Temperature 35.0 - 45.0 °C95.0 - 113 °FManual mixing
 35.0 - 45.0 °C95.0 - 113 °FHigh temperature machine
Gel Time 0.400 - 0.670 min0.400 - 0.670 minHigh temperature machine
 0.500 - 1.00 min0.500 - 1.00 minManual mixing
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceLight yellow transparent viscous liquid
Closed-cell rate=90%GB 10799
Cream time6-10 secHigh temperature machine
 8-16 secManual mixing
Dimensional stability=1.0%24h, -20?; GB/T8811
 =1.5%24h, 100?; GB/T8811
FlammabilityB2GB/T 8624
Hydroxyl value300-340 mgKOH/g
Recommended Ratio100:120-130DonPanel 422 blend polyols: Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM019 / 312548

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.