MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri CROSSVINIL EK/105 TI3 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Crossvinil: we have studied a special series of PVC compounds.

Crossvinil EK/105 TI3: special compound suitable for insulation and sheathing cables extrusion with interesting resistance to high temperature.

Certify: CEI 2011 TI3,BS 7655 TI3

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Tensile Strength >= 17.0 MPa>= 2470 psiISO R 527
 15.5 MPa
@Temperature 132 - 137 °C,
Time 1.21e+6 sec
2250 psi
@Temperature 270 - 279 °F,
Time 336 hour
Heat Ageing; IEC 60811
Elongation at Break >= 200 %>= 200 %ISO R 527
 >= 30 %
@Temperature -15.0 °C
>= 30 %
@Temperature 5.00 °F
Cold elongation
 190 %
@Temperature 133 - 137 °C,
Time 1.21e+6 sec
190 %
@Temperature 271 - 279 °F,
Time 336 hour
Heat Ageing; IEC 60811
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 90.0 °C194 °F<50%, penetration; IEC 60811
 
Processing PropertiesMetricEnglishComments
Zone 1 140 °C284 °F
Zone 2 150 °C302 °F
Zone 3 165 °C329 °F
Zone 4 180 °C356 °F
Die Temperature 195 °C383 °F
Head Temperature 190 °C374 °F
 
Descriptive Properties
Cold impact testno cracking, pass-15°C, IEC 60811
Exercise temperature90°C
Loss of mass<1.5 mg/cm²336 h @ 115 ± 2°C, IEC 60811
Thermal stability>240 min200°C, ISO R 182/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS003 / 294087

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.