  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin LS6010 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ LS6010 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high performance, injection moldable and extrudable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 1.5mm. NORYL LS6010 resin features low smoke production upon burning, high heat resistance, very low specific gravity, enhanced resistance to melting and dripping and meets the requirements of FAR 25.853. In addition, this material is heat stabilized and impact modified. It is an excellent candidate for aerospace interior applications such as rub strips, seat track covers, cable guides, switch panels, conduit, wall/ceiling mounted electronics, and parts machined from slab stock.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Moisture Absorption 0.0500 %0.0500 %23°C / 50% RH; ISO 62
 0.0700 %0.0700 %Profile Extrusion
 0.0700 %0.0700 %Sheet Extrusion
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Viscosity 5.0 cP
@Load 5.00 kg,
Temperature 280 °C
5.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 5.6 g/10 min
@Load 5.00 kg,
Temperature 280 °C
5.6 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psi50 mm/min; ASTM D638
 58.0 MPa8410 psi50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa9280 psi50 mm/min; ASTM D638
 64.0 MPa9280 psi50 mm/min; ISO 527
Elongation at Break 8.3 %8.3 %50 mm/min; ISO 527
 20 %20 %50 mm/min; ASTM D638
Elongation at Yield 4.6 %4.6 %50 mm/min; ASTM D638
 4.7 %4.7 %50 mm/min; ISO 527
Tensile Modulus 2.22 GPa322 ksi5 mm/min; ASTM D638
 2.44 GPa354 ksi1 mm/min; ISO 527
Flexural Strength 100 MPa14500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPa14500 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.36 GPa342 ksi2 mm/min; ISO 178
 2.39 GPa347 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 300 J221 ft-lbASTM D256
 181 J
@Temperature -30.0 °C
133 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²80*10*4; ISO 180/1A
 14.0 kJ/m²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 J38.4 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 143 °C289 °FRate B/50; ASTM D1525
 143 °C289 °FRate B/50; ISO 306
 146 °C295 °FRate B/120; ISO 306
Smoke Density  7.0
@Thickness 1.52 mm
7.0
@Thickness 0.0598 in
Non-Flaming, 4 min; ASTM E662
 30
@Thickness 1.52 mm
30
@Thickness 0.0598 in
Flaming, 4 min; ASTM E662
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 50.0 °C86.0 - 122 °FWater Bath Temperature
 30.0 - 60.0 °C86.0 - 140 °FCalibrator Temperature
Nozzle Temperature 295 - 305 °C563 - 581 °F
Zone 1 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
Zone 2 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
 290 - 300 °C554 - 572 °F
Zone 3 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
 295 - 305 °C563 - 581 °F
Zone 4 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
Adapter Temperature 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
Die Temperature 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
Melt Temperature 220 - 260 °C428 - 500 °FProfile Extrusion
 220 - 260 °C428 - 500 °FSheet Extrusion
 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 65.0 - 100 °C149 - 212 °F
Roll Temperature 90.0 - 150 °C194 - 302 °FRoll Stack Temp - Bottom
 90.0 - 150 °C194 - 302 °FRoll Stack Temp - Middle
 90.0 - 150 °C194 - 302 °FRoll Stack Temp - Top
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
 95.0 - 105 °C203 - 221 °FProfile Extrusion
 95.0 - 105 °C203 - 221 °FSheet Extrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 2.00 - 4.00 hour2.00 - 4.00 hourProfile Extrusion
 2.00 - 4.00 hour2.00 - 4.00 hourSheet Extrusion
 12.0 hour12.0 hourCumulative; Injection Molding
 12.0 hour12.0 hourCumulative; Profile Extrusion
 12.0 hour12.0 hourCumulative; Sheet Extrusion
Shot Size 30 - 70 %30 - 70 %
Screw Speed 40 - 80 rpm40 - 80 rpm
Precipitation Temperature 80.0 - 120 °C176 - 248 °FHopper Temperature
 
Descriptive Properties
Draeger Tube Toxicity, Flaming (1.52mm)PassASTM E662 - Modified
Draeger Tube Toxicity, Non-Flaming (1.52mm)PassASTM E662 - Modified
Flame Spread Index (1.52mm)15ASTM E162
Vertical Burn a (60s, 1.52mm) passes at0 SecondsFAR 25.853
Vertical Burn b (12s, 1.52mm) passes at4 SecondsFAR 25.853

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82345 / 290292

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.