MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC T7 AR Ceramic-Filled Industrial Barrier Coating
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: A novolac vinyl ester based, protective barrier coating for high temperature, chemical exposures where aggressive chemicals and abrasive conditions may be present.

ARC T7 AR industrial coating is designed to: Resist a wide range of inorganic, as well as organic acids and hydrocarbon based chemical compounds; Resist abrasion; Easily apply by trowel

Filler: A proprietary blend of high purity alumina ceramic reinforcements for resistance to sliding abrasion. Matrix: A flexibilized epoxy novolac vinyl ester resin reacted with a cumene hydrogen peroxide catalyst

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80ASTM D2240
Flexural Strength 22.4 MPa3250 psiASTM D790
Flexural Modulus 9.65 GPa1400 ksiASTM C580
Compressive Strength 71.77 MPa10410 psiASTM D695
Adhesive Bond Strength 15.51 MPa2249 psiPull-Off Adhesion; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °FWet Service
 180 °C356 °FDry Service
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 10.0 - 32.0 °C
6.00 Month
@Temperature 50.0 - 89.6 °F
Dry, Unopened Containers
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS037e / 239858

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.