Kaolite 2000-HS is a general-purpose, lightweight castable for use up to 2000°F (1093°C). It maintains excellent volume stability throughout its temperature use range. This is an excellent advantage for applications where strength and low thermal conductivity are required. Features: Light weight and low thermal conductivity reduce both the quantity of heat storage and heat transfer producing significant savings in furnace fuel consumptionLower densities reduce the amount of supporting furnace steelwork required and provide more insulation with a thinner lining. Applications: Backup insulation in two component linings in petrochemical process unitsHot face lining in ductwork from waste heat recovery boilers and process unitF.C.C.U. linings - regenerator.Hydrogen or reducing atmosphere linings Radiant section in steam flood generators.Hydrogen or reducing atmosphere linings.Steam flood generator convection sections and target wallsCat cracker regenerator liningsPetrochemical applicationsInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |