MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Spartech PP5140 Talc Filled Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperature

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/cc
@Temperature 22.8 °C
ASTM D792
Filler Content 40 %
Linear Mold Shrinkage 0.010 in/in0.125inch wall
 0.012 cm/cm4.0" disk; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4500 psiASTM D638
Elongation at Break 10 %ASTM D638
Elongation at Yield 2.0 %ASTM D638
Flexural Modulus 350000 psisecant; ASTM D790
 460000 psitangent; ASTM D790
Izod Impact, Notched 0.500 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact >= 1.00 ft-lb
@Temperature 22.8 °C
ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.8
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.7 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 172 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 175 °FASTM D648
Vicat Softening Point 84.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 20 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Drying Temperature 82.0 - 104 °C
Dry Time 4 - 6 hourto moisture < 0.01%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Spartech PP7140 Talc Filled High Impact Copolymer
Spartech PP5130 Talc Filled Homopolymer
Overview of materials for Polypropylene with 40% Talc Filler
Spartech EP5140 Talc Filled Homopolymer
Spartech PP7110 Talc Filled High Impact Copolymer

PSPAR112 / 78734

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.