MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group EP JS EPI Engineered Polymers Joint Sealant
Categories: Polymer; Thermoset

Material Notes: EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to protect interior horizontal concrete expansion and control joints from spalling, chipping, and breakdown. This elastomer displays fast cure times and excellent adhesion to concrete. EP JS can be applied at temperatures ranging -30° F to 350°F. This polyurea elastomer displays excellent chemical resistance, water insensitivity, and thermal stability at high and low temperatures. EP JS may also be used under traditional floor coatings (such as epoxies, polyureas and polyurethanes) or tiles to smooth the joints and provide protection from cracking and sinking caused by non-elastomeric joint sealants.

Applications:EP JS was designed to protect against the abuse to concrete joints caused by heavy load transfers from such items as forklifts, steel-wheeled carts and trash dumpsters. Some typical uses include:

  • Concrete Control / Expansion Joints
  • Concrete Spall Repairs
  • Cold Storage Facilities
  • Merchandise Distribution Centers
  • Home Improvement Stores
  • Bridge Headers
  • Warehouse Floors
  • D.O.T. Pothole Road Repair
  • U.S.D.A. and F.D.A. Acceptable
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Viscosity 400 cP2:1, A Side
     1200 cP2:1, B Side
     1200 cP1:1, Side B
     1800 cP1:1, Side A
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 851:1; ASTM D2240
     952:1; ASTM D2240
    Tensile Strength 1500 psi1:1; ASTM D412
     2950 psi2:1; ASTM D412
    Elongation at Break 350 %2:1; ASTM D412
     800 %1:1; ASTM D412
    100% Modulus 1.40 ksi
    @Strain 100 %
    0.0423611111111111; ASTM D412
     1.62 ksi
    @Strain 100 %
    0.0840277777777778; ASTM D412
    Adhesive Bond Strength >= 400 psiConcrete (no primer), Concrete Failure; ASTM D4541 Elcometer
    Tear Strength 450 pli1:1; ASTM D412
     500 pli2:1; ASTM D412
    Taber Abrasion, mg/1000 Cycles 20.51:1; CS17 Wheel, 1kg; ASTM D4060
     252:1; CS17 Wheel, 1kg; ASTM D4060
     
    Thermal PropertiesOriginal ValueComments
    Flash Point >= 200 °F2:1 and 1:1, ASTM Pensky-Martin
     
    Processing PropertiesOriginal ValueComments
    Tack-Free Time >= 0.0833 hourTack Free Time, 2:1
     >= 0.167 hourTack Free Time, 1:1
    Gel Time 2.00 min2:1
     5.00 min1:1
     
    Descriptive Properties
    ColorBlack, Gray
    Flexibility Pass2:1 and 1:1, ASTM D1737, 1/8"Mandrel
    Resistance to Acetic Acid (100%)Recommended
    Resistance to Clorox® (10%) H2OConditional, Discoloration
    Resistance to Diesel Fuel Recommended
    Resistance to GasolineRecommended
    Resistance to H2ORecommended
    Resistance to Hydraulic Fluid (oil) Recommended, Discoloration
    Resistance to Hydrochloric Acid (20%)Recommended
    Resistance to Hydrofluoric Acid(10%)Recommended, Discoloration
    Resistance to Mineral Spirits Recommended
    Resistance to Motor OilRecommended, Discoloration
    Resistance to Muriatic Acid (10%)Recommended
    Resistance to NaCl/H2O (10%)Recommended
    Resistance to Potassium Hydroxide (10%)Recommended
    Resistance to Sodium BicarbonateRecommended
    Resistance to Sodium Hydroxide (10%)Recommended
    Resistance to Sugar/H2ORecommended
    Resistance to Sulfuric Acid (>22%)Not Recommended
    Resistance to Sulfuric Acid (10%)Recommended, Discoloration
    Resistance to Vinegar/ H2O (5%)Recommended
    Resistance to Xylene Conditional

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    CHT Group EP LCP EPI Engineered Polymers Aromatic Polyurea
    Evonik TEGO® Antifoam 5-27 Emulsion
    Concrete, Highstrength
    CHT Group EP AJS EPI Engineered Polymers Aliphatic Joint Sealant
    BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)

    PACC105 / 22232

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.