MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teijin Tenax® E TPUD PEEK-HTS45 ThermoPlastic UniDirectional Prepreg
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Tenax®-E TPUD PEEK-HTS45 is a Thermoplastic Unidirectional prepreg (TPUD) which combines two high-performance materials. The polymer matrix of PEEK (polyetheretherketone) offers excellent resistance to chemicals and solvents and the utilization of Tenax®-E HTS45 a high tenacity carbon fiber manufactured with a tailored sizing for thermoplastics applications, result in a composite offering outstanding material performance.

Product Benefits

  • High-performance mechanical properties
  • Tailored thermoplastic sizing
  • Continuous use at elevated temperature
  • Low flammability, smoke and toxicity
  • Resistant to chemicals and solvents
  • Room temperature storage and shipping
  • Compliant to Health, Safety and Environment requirement
  • Recyclable
Process Benefits
  • Out of autoclave consolidation (press forming, vacuum bagging, filament winding)
  • Short cycle time
  • Thermo-formable
  • Automated process (AFP, ATL)
  • Thermoplastic joining technologies

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 88.0 MPa90°, 50 % r.h; DIN EN 2597 Type B
 2450 MPa0°, 50 % r.h; DIN EN 2561 Type A
Tensile Modulus 142 GPa0°, 50 % r.h; DIN EN 2561 Type A
Flexural Strength 1760 MPa0°, 50 % r.h; EN 2850 Type A3
Flexural Modulus 130 GPa0°, 50 % r.h; EN 2850 Type A3
Compressive Strength 1545 MPa0°, 50 % r.h; EN 2850 Type A3
Compressive Modulus 130 GPa0°, 50 % r.h; EN 2850 Type A3
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 143 °Conset, 50 % r.h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEIJIN919 / 277929

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.