MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Colmant Coated Fabrics Nitrile (NBR) Coated Cotton Tire Cord
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Tire cord fabric is a type of industrial fabric which is constructed using High Tenacity yarns in the warp direction and yarns of negligible resistance in weft direction which is used to hold warn yarns locked in their position. Tire cord coated fabrics provides fundamental properties such as controlled deformation, high strength, abrasion resistance, etc. Widely used by the tire industry, it is also employed for the rubber hose manufacture, air springs, expansion joints, among many other applications. Cotton is a natural fiber of vegetal origin. The cotton thread is derived from the transformation of Gossypium bristles (or cotton).Commonly we also referred under the same name the fabric after the weaving of the wire. Cotton is the first textile fiber used in the world despite the advent of synthetic fibers. It is inflamable and starts decomposition at 160 ° C. Cotton is popular thanks to its characteristics: aspect, lightness, comfort and ease of assembly and processing. NBR, as well known as Acrylonitrile Butadiene Rubber, was first developed in 1941 in a project meant to find an oil resistant rubber. However, NBR’s oil resistance depends on the grade of acrylonitrile. The higher the grade of acrylonitrile the better is resistance to oil and fuel. However, as the grade of acrylonitrile increases, the endurance to low temperatures decreases. NBR has good abrasion resistance nonetheless its physical properties are moderate in comparison with the Natural Rubber.

Applications:

  • Expansion joints
  • shutters
  • inflatable pipe plugs and lifting bags
Properties:
  • Fireproofed
  • Non-skid
  • Oil storage
  • Fuel storage
  • Cold resistance

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 90
Tensile Strength at Break 8.00 - 20.0 MPa
Elongation at Break 100 - 900 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 115 °C
Minimum Service Temperature, Air -20.0 °C
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-20 C° - 120°C
Warp breaking strength75 - 120 daN/5cm
Warp elongation at break10% - 20%
Weft breaking strength70 - 90 daN/5cm
Weft elongation at break10% - 20%
Weight per sqm200 - 400

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLMANT031 / 316081

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.