MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting tool applications that require an optimum balance of red hardness, edge toughness and wear resistance. The combination of outstanding properties and high hardness response makes Tatmo-VN a logical alternative for cobalt high speed steels in may cutting tool applications. Typical applications for Tatmo-VN high speed steel include twist drills, taps, end mills, reamers and milling cutters.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.94 g/cc
Density 0.287 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 59Oil Quenched at 1218°C; 622°C Temper Temperature
 63Oil Quenched from 1191°C; 482°C Temper Temperature
 63Oil Quenched from 1191°C; 482°C Temper Temperature
 63.5Oil Quenched at 1218°C; 482°C Temper Temperature
 66.1Oil Quenched from 1191°C; 538°C Temper Temperature
 66.5Oil Quenched at 1218°C; 538°C Temper Temperature
Modulus of Elasticity 30000 ksi
Machinability 45 - 50 %1% Carbon Steel
Izod Impact Unnotched 21.0 ft-lbOil Quenched at 1218°C; 482°C Temper Temperature
 24.0 ft-lbOil Quenched at 1218°C; 594°C Temper Temperature
 27.0 ft-lbOil Quenched at 1218°C; 622°C Temper Temperature
 29.0 ft-lbOil Quenched at 1191°C; 594°C
 31.0 ft-lbOil Quenched at 1191°C; 482°C
 39.0 ft-lbOil Quenched at 1191°C; 622°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.68 µm/m-°C
@Temperature 21.0 - 204 °C
 13.3 µm/m-°C
@Temperature 21.0 - 538 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 749 °CCritical Temperaure Ar3
 780 °CCritical Temperaure Ar1
 824 °CCritical Temperaure Ac1
 860 °CCritical Temperaure Ac3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.02 %
Chromium, Cr 3.75 %
Iron, Fe 82.53 %
Manganese, Mn 0.25 %
Molybdenum, Mo 8.5 %
Silicon, Si 0.30 %
Tungsten, W 1.75 %
Vanadium, V 1.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe HS-29XL™ ASTM M2-HC High Speed Steel
AISI 1005 Steel
Latrobe Tatmo-V™ AISI M7 High Speed Steel
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Aluminum, Al

NTIMK068 / 19415

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.