MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell PMA Propylene glycol methyl ether acetate
Categories: Fluid; Solvent

Material Notes: Available in electronic grade.

Information provided by Lyondell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.969 g/cc
@Temperature 20.0 °C
20/20°C
Density 0.959 g/cc
@Temperature 20.0 °C
Solubility in Water 18 %20°C
Viscosity 1.1 cP
@Temperature 25.0 °C
Molecular Weight 132.2 g/mol
Vapor Pressure 2.80 torr
@Temperature 20.0 °C
Evaporation Loss 34 %n-BuAc=100%
Surface Tension 27 dynes/cm25°C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 140 °Cat 760 mmHg
Flash Point 47.0 °CTag Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.40
@Temperature 25.0 °C
 
Descriptive Properties
CAS Number108-65-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell PM Propylene glycol methyl ether
LyondellBasell Hifax EKC 177P BLACK Polypropylene
Overview of materials for PVC, Flexible Grade
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Omni Plastics OmniTech™ PMA IM UV PMMA

WLYON14 / 76282

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.