Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This product is fully colorable and is available in both UV-stabilized and non-UV-stabilized options. It is most functional when used as substrate layer for INDURE® E1500HG to provide a structure with excellent cold temperature impact properties as well as high stiffness. Applications: Substrate layer for E1500HG high gloss cap layer or general purpose monolith material for sheet extrusion and thermoforming. Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line. |