MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protection and show excellent "crush strength." Hipscon maintains extremely low gloss surfaces after forming, allowing for easy reading of package contents via automated sensors. Hipscon™ M-520 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish.

Features:

  • Superior crush strength
  • High degree of stiffness
  • Uniform pocket formation
  • Consistent, permanent ESD protection

Applications:

  • Electronic component packaging and handling trays
  • Tape & reel
  • Material handling boxes and bins

Data provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.1 MPa3500 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Tensile Modulus 1.86 GPa270 ksiASTM D638
Flexural Modulus 1.86 GPa270 ksiInjection Molded; ASTM D790-92
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cmASTM D257
Surface Resistance <= 1e+05<= 1e+05ASTM D257
Static Decay <= 0.010 sec<= 0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 <= 0.010 sec<= 0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 12 %12 %60°; Front
 12 %12 %60°; Back
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane

PNOVEON04 / 55306

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.