MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

NOVA Chemicals SURPASS® HPs 167-AB sHDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Homopolymer

Features:

  • Superior barrier properties
  • Very high stiffness
  • Low gel

Additives:

  • Processing antioxidant

Applications:

  • Moisture barrier films
  • Co-extrusion
  • Dry food packaging

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 100-mil die gap at a blow up ratio of 2:1, but are dependent upon operating conditions.

United States: SURPASS HPs167-AB resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.2, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.967 g/cc0.0349 lb/in³ASTM D 792
Water Vapor Transmission 1.10 g/m²/day
@Temperature 38.0 °C
0.0708 g/100 in²/day
@Temperature 100 °F
100% RH; ASTM F 1249
Oxygen Transmission Rate 465 cc/m²/day
@Temperature 23.0 °C
29.9 cc/100 in²/day
@Temperature 73.4 °F
0% RH; ASTM D 3985
Thickness 38.0 microns1.50 mil
Melt Index of Compound 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 27.0 MPa3920 psiASTM D 882
Film Tensile Strength at Yield, TD 25.0 MPa3630 psiASTM D 882
Elmendorf Tear Strength MD 22 g22 gASTM D 1922
Elmendorf Tear Strength TD 225 g225 gASTM D 1922
1% Secant Modulus, MD 1100 MPa160000 psiASTM D 882
1% Secant Modulus, TD 1335 MPa193600 psiASTM D 882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)19NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVB102 / 194710

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.