MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Pamolyn™ 200 Linoleic Acid
Categories: Fluid

Material Notes: Product Description: Pamolyn™ 200 linoleic acid is a high purity grade of linoleic acid derived wholly from a tall oil fatty acid source. It is a pale, oily liquid with low odor, and is highly resistant to discoloration on exposure to heat and light. Because of the near absence of saturated fatty acids, this product has exceptionally low titer. Pamolyn™ 200 linoleic acid contains a low percentage of unsaponifiables and resin acids. Pamolyn™ 200 linoleic acid is designed especially for the protective coatings industry for production of pale, color retentive, fast drying alkyds and epoxy resin ester coatings. Other uses for this linoleic acid are in applications that require both wetting and drying properties, such as printing ink vehicles and caulking and sealant compositions.

Application/Uses:

  • Building and Construction
  • Caulks and Sealants
  • Graphic Arts
  • Hot Melt Adhesives
  • Paint and Coatings
  • Solventborne Adhesives
Key Attributes:
  • High purity, low odor, pale color linoleic acid
  • Highly resistant to discoloration on exposure to heat and light
  • Low rosin acid content
  • Low unsaponifiables
  • Very low titer point

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.904 g/cc
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 193
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 3.5
 
Descriptive Properties
Colorafter heat test, D 1981-61
Saponification Number196

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5479 / 222673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.