MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Acenaphthylene
Material Notes: Enthalpy of sublimation, 17.0 kcal/mol at 298 K; Henry's Law constant = 1.25X10-4 atm-cu m/mol at 25°C; Hydroxyl radical reaction rate constant = 1.09X10-10 cu cm/molec-sec at 25°C; Gas-phase ozone reaction rate constant = 3.99-16 cu cm/molec-sec at 25°C; Nitrate radical reaction rate constant = 4.42X10-12 cu cm/molec-sec at 25°C

Storage: Stable under recommended storage conditions.

Applications: Polycyclic aromatic hydrocarbons are carcinogenic

ACENAPHTHYLENE is a colorless crystalline solid. Insoluble in water. Used in dye synthesis, insecticides, fungicides, and in the manufacture of plastics.

Synonyms: Tox21_300587; MFCD00003806; 208-96-8; InChI=1/C12H8/c1-3-9-4-2-6-11-8-7-10(5-1)12(9)11/h1-8; FT-0600515; Cyclopenta[de]naphthalene; RTR-009826; TRA0083522; G00031-Watson-Int; NSC-59821

Smiles: C1=CC2=C3C(=C1)C=CC3=CC=C2;

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.8987 g/cc
@Temperature 16.0 °C
0.03247 lb/in³
@Temperature 60.8 °F
Molecular Weight 152.063 g/mol152.063 g/mol"Exact Mass" - Based on Specific Isotopes
 152.063 g/mol152.063 g/molMonoisotopic Mass - Isotopic Peak from Most Abundant Isotopes
 152.196 g/mol152.196 g/mol
Vapor Pressure 0.00000640 bar
@Temperature 25.0 °C
0.00480 torr
@Temperature 77.0 °F
Storage Temperature 4.00 °C39.2 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 89.4 °C193 °F
 
Descriptive Properties
Alfa Chemistry Materials CategoryPolymer Science
CAS Number208-96-8
Color/FormYellow needles; Colorless crystalline solid; Prisms from ether and plates from alcohol;
Complexity184
Covalently-Bonded Unit1
DecompositionHazardous decomposition products formed by heat or fire - Carbon oxides.
 When heated to decomposition, it emits acrid smoke and irritating fumes.
EC Number205-917-1
Heavy Atom Count12
InChIInChI=1S/C12H8/c1-3-9-4-2-6-11-8-7-10(5-1)12(9)11/h1-8H;
InChIKeyHXGDTGSAIMULJN-UHFFFAOYSA-N;
IUPAC Nameacenaphthylene;
Molecular FormulaC12H8
NSC Number59821
Octanol/Water Partition Coefficient3.94 (LogP);log Kow = 3.93;
SolubilityInsoluble In water
 Slightly soluble in chloroform
 Very soluble in ethanol, ether, benzene
StabilityStable under recommended storage conditions.
Topological Polar Surface Area0A^2
UN Number3077
UNII1Z25C36811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA1921 / 270014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.