MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Clyrell RC 213M Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC213M is a high flow and highly modified polypropylene random copolymer. It   contains anti-blocking additives. It does not contain Calcium Stearate. Clyrell RC213M is typically used for manufacturing of oriented and un-oriented films. Typical applications reported by customers are lamination, metalized films, textile and packaging of foodstuffs. In addition, customers also reported that it is particularly suitable as a skin of multilayer twist film. Customers have been reporting that films produced using Clyrell RC213M offer a good balance of properties such as high clarity, brightness, stiffness and medium seal initiation temperature (SIT). Applications: Barrier Film, Food Packaging Film, Twist Wrap Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 22.0 MPaASTM D882
Film Elongation at Break, MD 750 %ASTM D 882
Coefficient of Friction 1.0ASTM D 1894
Film Tensile Strength at Break, MD 35.0 MPaASTM D882
1% Secant Modulus, MD 660 MPa
@Thickness 0.0500 mm
30mm/min; ASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %
@Thickness 0.0500 mm
ASTM D1003
Gloss 90 %
@Thickness 0.0500 mm
ASTM D 2457
 
Descriptive Properties
Processing MethodBOPP, Cast Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adsyl™ 5 C 30 F Polyolefin
LyondellBasell Adsyl™ 3 C 30 F HP Polypropylene Copolymer
LyondellBasell Adsyl 7641 XCP Polypropylene terpolymer
LyondellBasell Clyrell RC 211M Polypropylene
Arkema OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene

PEQT7086 / 218724

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.