It can be used on partially stabilized zirconia and tape cast Materials. The Platinum powder contained within this paste has low shrinkage and high adhesion to ceramic substrates. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156-325 tpi Substrate: Partially stabilized zirconia and tape cast MaterialsInformation provided by Gwent Electronic Materials Ltd. |