MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® 58201 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.

Features: Tear resistant properties.

Uses: Injection Molding and general extrusion techniques.

Available in Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282ASTM D2240
Tensile Strength 39.0 MPa5660 psiASTM D412; ASTM D638
Elongation at Break 680 %680 %ASTM D412; ASTM D638
50% Modulus 3.80 MPa
@Strain 50 %
3.80 MPa
@Strain 50 %
ASTM D412; ASTM D638
100% Modulus 4.60 MPa
@Strain 100 %
667 psi
@Strain 100 %
ASTM D412; ASTM D638
300% Modulus 7.10 MPa
@Strain 300 %
1030 psi
@Strain 300 %
ASTM D412; ASTM D638
Rebound 1.0 %1.0 %DIN 53512
Tear Strength 44.0 kN/m251 pliDie C; ASTM D624
Abrasion 4343mm3; DIN 53516
Compression Set  28 %
@Temperature 23.0 °C,
Time 79200 sec
28 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 71 %
@Temperature 70.0 °C,
Time 79200 sec
71 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -70.0 °C-94.0 °FDIN 53546

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Envalior TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate

PNOVEON557 / 121448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.