MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes: The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccISO 1183
Water Absorption at Saturation 0.20 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89DIN 53505
Ball Indentation Hardness 130 MPa
Tensile Strength at Break 100 MPaISO 527
Elongation at Break 1.5 %ISO 527
Modulus of Elasticity 8.00 GPaISO 527
Flexural Strength 125 MPaISO 178
Charpy Impact Unnotched 25.0 kJ/m²ISO 179
Charpy Impact, Notched 8.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmVDE 0303
Surface Resistance >= 1.00e+13 ohm
Dielectric Constant 2.9
@Frequency 1e+6 Hz
Dielectric Strength 18.0 kV/mmVDE 0303
Dielectric Loss Index 0.0010
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CDIN 53752
Thermal Conductivity 0.280 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 110 °C
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 140 °CISO 75
Vicat Softening Point 145 °CVST/B/50; ISO 306
 155 °CVST/A/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-1UL 94
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceno
Bondabilityyes
CKW Resistanceno
Hydrocarbonate Resistancelimited
Hydroxide Resistanceyes
Ketone Resistanceyes
Resistance Against Hot Wateryes
UV Stabilizationfair

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestoran® 1300-GF30 nf PPE
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber
GEHR Plastics PSU Polysulfone
BLUESTAR LXS 314 G40 PPE-HIPS, 40% Glass Filled
Asahi Kasei Xyron™ G703H PPE/PS, Glass Fiber Reinforced

PGEHR015 / 79852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.