MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Space Grade, Low modulus urethane ESD coating/adhesive
APTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an electrostatic charge. This low-outgassing system provides a combination of high flexibility and good tensile strength/elongation characteristics.

Capable of full cure at RT for application where heat cure is not desired or possible; Exceeds NASA outgassing requirements for space applications; Non-TDI based for safety; Excellent version resistance for good physical stability under high heat and humidity environments; Tg below -60ºC for excellent low temperature cycling, storage and performance; Excellent substrate adhesion; superior to silicones; Available in pre-measured kits to minimize handling

APTEK 2214A is a black carbon-filled polyol resin. APTEK 2214B is a pale yellow organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccA Component; ASTM D1475
 1.22 g/ccB Component; ASTM D1475
Viscosity 40 cPB Component; ASTM D1824
Outgassing - Total Mass Loss 0.59 %Cured property; at 10E-6 torr; ASTM E-595
Collected Volatile Condensable Material 0.040 %Cured property; at 10E-6 torr; ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70Cured property; ASTM D2240
Tensile Strength, Ultimate 450 psiCured property; ASTM D412
Elongation at Break 300 %Cured property; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 3.50e+6 ohmCured property; ETS 860B
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg <= -60.0 °CCured property; Perkin Elmer TS-2
Flash Point >= 10.0 °CA Component; ASTM D92
 >= 200 °CB Component; ASTM D92
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °CCure 168 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Allnex UCECOAT® 2501 Waterborne UV Resin
Aptek DIS-A-PASTE 2000-A/B Thermally conductive urethane adhesive
BASF Ultramid® A3WG6 LS BK 23189 30% Glass Filled PA66 (Conditioned)
Lord Adhesives CoolTherm™ EP-6968 Conductive Adhesive System
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer

PAPTEK12 / 24174

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.