MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical GYC-AT-110 Antistatic Agent with High Transparency
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GYC-AT-110 is a highly transparent antistatic agent which is developed by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP). It is widely used in manufacturing products that transparent appearance is required, for it exhibits high transparency, great heat stability, and superior quality. GYCAT-110 provides exceptional antistatic performance and is applied to PP, PE, PVC, LDPE, acrylic, ABS, PA, PC, POM, HIPS, EPS, PTR, phenolic resin, thermosetting plastic, thermoplastic, resin, elastomer, general plastic, engineering plastic, etc. It is also used in the spinning of nylon fiber to avoid broken course.

Advantages:

  • Provides exceptional antistatic performance
  • With high transparency
  • Features great heat stability, and superior quality
  • Effectively reduces the surface resistance value
  • Can be used for the applications of extrusion molding, injection molding, and blown film
  • Excellent dispersivity and the efficiency of compounding
Applications:
  • Thermosetting plastic, thermoplastic, resin
  • General plastic, engineering plastic
  • PP, PE, PVC, LDPE
  • Acrylic, ABS, PA, PC, POM, HIPS
  • EPS, TPR, phenolic resin
  • Rubber product
  • Spinning of nylon fiber
  • Paint/coating, powder coating
  • Can be made into antistatic masterbatch and be used in plastic

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 °C293 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
AppearanceSolid
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN258 / 266566

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.