MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, Conditioned  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick.

Availability:

  • Asia Pacific
  • Europe
  • North America
Additive:
  • Halogen
  • Lubricant
Features:
  • Ductile
  • Flame Retardant
  • Good Crack Resistance
  • Good Mold Release
  • Good Toughness
  • Halogenated
  • High Elongation
  • Ignition Resistant
  • Low Density
  • Lubricated
Uses:
  • Appliances
  • Automotive Electronics
  • Bobbins
  • Connectors
  • Electrical Housing
  • Electrical Parts
  • Electrical/Electronic Applications
  • Fasteners
  • Industrial Applications
  • Lighting Applications
  • Living Hinges
  • Printed Circuit Boards
  • Switches
Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.9 %1.9 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Diameter 2.00 mm
0.013 in/in
@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm
@Diameter 2.00 mm
0.018 in/in
@Diameter 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psiISO 527-2
Elongation at Break 75 %75 %ISO 527-2
Elongation at Yield 25 %25 %ISO 527-2
Tensile Modulus 2.30 GPa334 ksiISO 527-2
Flexural Strength 43.0 MPa6240 psiISO 178
Flexural Modulus 1.40 GPa203 ksiISO 178

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZVYDYM901 / 177252

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.