MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Bioline 4C27A Free-cutting wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik Bioline 4C27A is a hardenable stainless chromium steel alloyed with molybdenum. This grade is supplied in wire form. It is characterized by:
  • Very good machinability
  • High wear resistance
  • Good toughness
  • Good corrosion resistance due to addition of molybdenum
Sandvik Bioline 4C27A is used for the manufacture of precision components such as watch parts, measuring points, dental tools, precision instruments and drilled surgical needles.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  <= 800 MPa
@Diameter 0.600 - 3.00 mm
<= 116000 psi
@Diameter 0.0236 - 0.118 in
Wire in coils, Annealed
 <= 800 MPa
@Diameter 0.600 - 10.0 mm
<= 116000 psi
@Diameter 0.0236 - 0.394 in
Straightened wire, Annealed
 <= 800 MPa
@Diameter 0.600 - 10.0 mm
<= 116000 psi
@Diameter 0.0236 - 0.394 in
Straightened wire, Annealed
 850 MPa
@Diameter 5.00 - 10.0 mm
123000 psi
@Diameter 0.197 - 0.394 in
Straightened wire, Drawn/ground
 850 MPa
@Diameter 5.00 - 10.0 mm
123000 psi
@Diameter 0.197 - 0.394 in
Straightened wire, Drawn
 950 MPa
@Diameter 0.600 - 3.00 mm
138000 psi
@Diameter 0.0236 - 0.118 in
Straightened wire, Drawn/ground
 950 MPa
@Diameter 3.00 - 5.00 mm
138000 psi
@Diameter 0.118 - 0.197 in
Straightened wire, Drawn/ground
 950 MPa
@Diameter 0.600 - 3.00 mm
138000 psi
@Diameter 0.0236 - 0.118 in
Straightened wire, Drawn
 950 MPa
@Diameter 3.00 - 5.00 mm
138000 psi
@Diameter 0.118 - 0.197 in
Straightened wire, Drawn
 950 MPa
@Diameter 0.450 - 4.00 mm
138000 psi
@Diameter 0.0177 - 0.157 in
Wire in coils, Drawn
Tensile Strength, Yield  >= 450 MPa
@Diameter 0.600 - 3.00 mm,
Strain 0.2 %
>= 65300 psi
@Diameter 0.0236 - 0.118 in,
Strain 0.2 %
Wire in coils, Annealed
 >= 450 MPa
@Diameter 0.600 - 10.0 mm,
Strain 0.2 %
>= 65300 psi
@Diameter 0.0236 - 0.394 in,
Strain 0.2 %
Straightened wire, Annealed
 >= 450 MPa
@Diameter 0.600 - 10.0 mm,
Strain 0.2 %
>= 65300 psi
@Diameter 0.0236 - 0.394 in,
Strain 0.2 %
Straightened wire, Annealed
 >= 650 MPa
@Diameter 5.00 - 10.0 mm,
Strain 0.2 %
>= 94300 psi
@Diameter 0.197 - 0.394 in,
Strain 0.2 %
Straightened wire, Drawn/ground
 >= 650 MPa
@Diameter 5.00 - 10.0 mm,
Strain 0.2 %
>= 94300 psi
@Diameter 0.197 - 0.394 in,
Strain 0.2 %
Straightened wire, Drawn
 >= 700 MPa
@Diameter 0.450 - 4.00 mm,
Strain 0.2 %
>= 102000 psi
@Diameter 0.0177 - 0.157 in,
Strain 0.2 %
Wire in coils, Drawn
 >= 770 MPa
@Diameter 0.600 - 3.00 mm,
Strain 0.2 %
>= 112000 psi
@Diameter 0.0236 - 0.118 in,
Strain 0.2 %
Straightened wire, Drawn
 >= 770 MPa
@Diameter 3.00 - 5.00 mm,
Strain 0.2 %
>= 112000 psi
@Diameter 0.118 - 0.197 in,
Strain 0.2 %
Straightened wire, Drawn
 >= 770 MPa
@Diameter 0.600 - 3.00 mm,
Strain 0.2 %
>= 112000 psi
@Diameter 0.0236 - 0.118 in,
Strain 0.2 %
Straightened wire, Drawn/ground
 >= 770 MPa
@Diameter 3.00 - 5.00 mm,
Strain 0.2 %
>= 112000 psi
@Diameter 0.118 - 0.197 in,
Strain 0.2 %
Straightened wire, Drawn/ground
Elongation at Break  10 %
@Diameter 0.600 - 3.00 mm
10 %
@Diameter 0.0236 - 0.118 in
Straightened wire, Drawn
 10 %
@Diameter 3.00 - 5.00 mm
10 %
@Diameter 0.118 - 0.197 in
Straightened wire, Drawn
 10 %
@Diameter 0.450 - 4.00 mm
10 %
@Diameter 0.0177 - 0.157 in
Wire in coils, Drawn
 10 %
@Diameter 0.600 - 3.00 mm
10 %
@Diameter 0.0236 - 0.118 in
Straightened wire, Drawn/ground
 10 %
@Diameter 3.00 - 5.00 mm
10 %
@Diameter 0.118 - 0.197 in
Straightened wire, Drawn/ground
 11 %
@Diameter 5.00 - 10.0 mm
11 %
@Diameter 0.197 - 0.394 in
Straightened wire, Drawn/ground
 11 %
@Diameter 5.00 - 10.0 mm
11 %
@Diameter 0.197 - 0.394 in
Straightened wire, Drawn
 25 %
@Diameter 0.600 - 10.0 mm
25 %
@Diameter 0.0236 - 0.394 in
Straightened wire, Annealed
 25 %
@Diameter 0.600 - 10.0 mm
25 %
@Diameter 0.0236 - 0.394 in
Straightened wire, Annealed
 25 %
@Diameter 0.600 - 3.00 mm
25 %
@Diameter 0.0236 - 0.118 in
Wire in coils, Annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.5 µm/m-°C
@Temperature 30.0 - 100 °C
5.83 µin/in-°F
@Temperature 86.0 - 212 °F
Cold drawn
 11.0 µm/m-°C
@Temperature 30.0 - 200 °C
6.11 µin/in-°F
@Temperature 86.0 - 392 °F
Cold drawn
 11.0 µm/m-°C
@Temperature 30.0 - 100 °C
6.11 µin/in-°F
@Temperature 86.0 - 212 °F
Heat treated
 11.5 µm/m-°C
@Temperature 30.0 - 200 °C
6.39 µin/in-°F
@Temperature 86.0 - 392 °F
Heat treated
 11.5 µm/m-°C
@Temperature 30.0 - 300 °C
6.39 µin/in-°F
@Temperature 86.0 - 572 °F
Heat treated
 11.5 µm/m-°C
@Temperature 30.0 - 300 °C
6.39 µin/in-°F
@Temperature 86.0 - 572 °F
Cold drawn
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.22 %0.22 %
Chromium, Cr 13 %13 %
Manganese, Mn 1.3 %1.3 %
Molybdenum, Mo 1.2 %1.2 %
Nickel, Ni 0.80 %0.80 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.60 %0.60 %
Sulfur, S 0.20 %0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5185 / 199749

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.