MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAMID® 66 HS PA 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product characteristics:
  • Good heat ageing resistance
  • Good thermal stability
  • Good dimensional stability
Product applications:
  • Mechanical engineering
  • Transpiration industry
  • Steel industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN EN ISO 1183-1
Water Absorption 2.8 %2.8 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282DIN EN ISO 868
Tensile Strength, Yield 85.0 MPa12300 psiDIN EN ISO 527
Elongation at Break 50 %50 %DIN EN ISO 527
Modulus of Elasticity 3.30 GPa479 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmDIN EN 62631-3-2
Dielectric Constant 3.83.8IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243
Dissipation Factor 0.015
@Frequency 50 Hz
0.015
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN 53752
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FDIN 52612
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 260 °C500 °FISO 11357-3
Maximum Service Temperature, Air 120 °C248 °Flong term
 170 °C338 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FDIN EN ISO 75
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 V-2
@Thickness 6.00 mm
V-2
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ GF30 / Ertalon™ 66 GF30 PA66 30% glass filled, extruded
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
EPICHEM PA 66 Polyamide 66
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
EPICHEM Epinyl PA 66 Polyamide 66

PROCH9305 / 233007

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.