MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vinnolit® E 68 SA PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 68 SA PVC for paste application. Vinnolit® E 68 SA is a fine-particle paste making emulsion homopolymer, classified as a low to medium viscosity resin. Plastisols made with Vinnolit® E 68 SA exhibit a nearly Newtonian rheology. Vinnolit® E 68 SA is recommended for the production of chemically blown foams. Typical applications are for example artificial leather, floorings, unsupported foams and foamed wallcoverings. Noteworthy properties are: low to medium viscosity, excellent foaming characteristics with good expansion ratio and a uniform, fine cell structure, even at high filler loading, readily blended with Vinnolit® C 65 V or Vinnolit® EXT up to a ratio of 60/40 to obtain rigid or semi-rigid foams without sacrificing cell structure, very good whiteness, good paste deaeratibility, wide processing tolerance with no tendency to overfoaming.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.30 %<= 0.30 %ISO 1269
Apparent Bulk Density 0.440 g/cc0.0159 lb/in³ISO 60
Particle Size <= 63 µm<= 63 µm<= 3.0% Retained on 0.063 mm Sieve; DIN EN ISO 53195
Viscosity Test 116 cm³/g1.16 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentMedium
K-Value68ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO946 / 291143

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.