MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GY-IM 100 Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GY-IM100 SERIES, one of super modifier of owning fiberplastic functions, developed & manufactured by GO YEN CHEMICAL INDUSTRIAL CO. LTD. and co-cooperation with GGK company. GY-IM100 SERIES are used for various kinds of polymer industries and can enhance not only the chemical property but also physical functions, including weather-resistant, impact-resistant, strong elongation strength, excellent durability of low temperature and good optical capacity. GY-IM100 participation will offer high additive value for your products & increasing competitiveness. It obtains a good reputation from many larger plastic and fiber producers in Japan, Korea, Europe & American countries.

Applications:

  • ABS – Acrylonitrile-Butadine-Styrene
  • PE,PP,EVA – Polyethylene & Polyolefin
  • Fiber polymer – Nylon fiber , PET Fiber, PP fiber
  • PS – Poly styrene
  • PVC – Poly Vinyl chloride
  • ASA – Acrylonitrile- Styrene -Acrylate
  • PC – Polycarbonate
  • Elastomer – TPU,TPE-TPR(SBS,SEBS,SIS)…..ETC
  • Rubber – NR,CR,EPDM…….ETC
  • Engineer Plastic – PA , PBT , PET , And Additive GF Grade
  • Master batch & Other Special Application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.25 %0.25 %
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 750 %>= 750 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN299 / 266607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.