Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness. Features: 40% Glass Reinforced, Halogen free, Chlorine Content < 900 ppm. Processing: Injection molding. Former DSM Engineering Plastics product line is now with Envalior. |