MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
3M Techical Ceramics MYCROSINT® CD Boron Nitride
Categories: Ceramic; Carbide

Material Notes:

Information provided by 3M Technical Ceramics, formerly ESK Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 1.97 g/ccAnisotropic, Perpendicular; DIN EN 623-2
 >= 1.97 g/ccAnisotropic, Parallel; DIN EN 623-2
Porosity <= 12 %Anisotropic, Perpendicular; DIN EN 623-2
 <= 12 %Anisotropic, Parallel; DIN EN 623-2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 13Anisotropic, Perpendicular; DIN EN ISO 6506-1
 13Anisotropic, Parallel; DIN EN ISO 6506-1
Tensile Modulus 25.0 GPaYoung's, Anisotropic, Parallel; DIN EN 843-2
 30.0 GPaYoung's, Anisotropic, Perpendicular; DIN EN 843-2
Flexural Strength 35.0 MPaAnisotropic, Parallel; DIN EN 843-1
 40.0 MPaAnisotropic, Perpendicular; DIN EN 843-1
Compressive Strength 50.0 MPaAnisotropic, Perpendicular; AAW/AC-R-302-03
 55.0 MPaAnisotropic, Parallel; AAW/AC-R-302-03
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cmAnisotropic, Perpendicular
 >= 1.00e+12 ohm-cmAnisotropic, Parallel
 
Thermal PropertiesOriginal ValueComments
CTE, linear -1.00 µm/m-°C
@Temperature 20.0 - 500 °C
Anisotropic, Perpendicular; DIN EN 821-1
 -1.00 µm/m-°C
@Temperature 20.0 - 500 °C
Anisotropic, Parallel; DIN EN 821-1
 1.50 µm/m-°C
@Temperature 500 - 1000 °C
Anisotropic, Perpendicular; DIN EN 821-1
 2.00 µm/m-°C
@Temperature 500 - 1000 °C
Anisotropic, Parallel; DIN EN 821-1
 3.00 µm/m-°C
@Temperature 1000 - 1500 °C
Anisotropic, Perpendicular; DIN EN 821-1
 4.00 µm/m-°C
@Temperature 1000 - 1500 °C
Anisotropic, Parallel; DIN EN 821-1
Specific Heat Capacity 0.580 J/g-°CAnisotropic, Perpendicular
 0.580 J/g-°CAnisotropic, Parallel
Thermal Conductivity 35.0 W/m-KAnisotropic, Perpendicular
 35.0 W/m-KAnisotropic, Parallel
Maximum Service Temperature, Air 1100 °COxidizing, Anisotropic, Perpendicular
 1100 °COxidizing, Anisotropic, Parallel
Maximum Service Temperature, Inert 1500 °CAnisotropic, Perpendicular
 1500 °CAnisotropic, Parallel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials HBR Hot-Pressed Boron Nitride
Silicon Carbide, Reaction-Bonded, SiSiC
Thermal Transfer Composites PRIMEX ULTRA™ MCT-587™ Aluminum Silicon Carbide Composite, Reinforced
3M Techical Ceramics MYCROSINT® HD Boron Nitride
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)

CESK16 / 183308

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.