Description: - Flexible, loaded nitrile rubber based microwave absorber.
- ND-12034 is tuned for mode suppression in an enclosed cavity, signal isolation and surface current attenuation.
- Standard sheet size: 24” x 24” (30.48 cm x 30.48 cm); Custom sizes available upon request.
- ND-12034 comes with pressure sensitive adhesive (PSA).
- Can be water-jet or die cut for custom configurations.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |