MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: COPYLENE™ CH034, a polypropylene homopolymer resin, is designed for the production of biaxially oriented polypropylene films (BOPP). Potential uses include metalized film applications, (either directly or as core layer of coextruded film), other BOPP packaging films, and Solid Phase Thermoforming sheet. The material contains standard processing stabilization but does not contain any slip or antiblocking agents and is Calcium Stearate free. COPYLENE™ CH034 offers good optical properties, easy processing and a very good film profile. Applications: Bags & Pouches, Raffia/Tapes/Strapping, Peelable Film, Film Wrap, Food Packaging Film, Lamination Film, Twist Wrap Film, Surface Protection Film, Barrier Film. Equivalent to Pro-fax® HL451J

Information provided by Phillips 66.

Key Words: Designed for BOPP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 3.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.1 MPa4800 psi2 in/min; ASTM D638
Elongation at Yield 12 %12 %ASTM D638
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chengdu Polyster PP Film PP Films/Sheets
Dow LDPE 493A Low Density Polyethylene, Film Grade
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film
Formosa Plastics Formolene® 1102K Cast and BOPP Film Polypropylene
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade

PCOPY012 / 100808

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.