MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 440 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 440 is a nominal 40 Shore D thermoplastic polyester elastomer with medium modulus.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cmISO 294-4
Melt Flow 13.3 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868
Hardness, Shore D 3815 sec; ISO 868
 38ISO 868
Tensile Strength at Break 18.0 MPa50mm/min; ISO 527-2/1A
 21.0 MPaISO 527-1/2
Tensile Stress at Strain 2.00 MPa
@Strain 5.0 %
ISO 527-1/2
 4.00 MPa
@Strain 10 %
ISO 527-1/2
 7.00 MPa
@Strain 50 %
ISO 727-1/2
 7.00 MPa
@Strain 50 %
ISO 527-2/1A
 8.00 MPa
@Strain 100 %
ISO 527-1/2
 12.7 MPa
@Strain 300 %
ISO 527-1/2
Elongation at Break 650 %50mm/min; ISO 527-2/1A
 650 %ISO 527-1/2
Tensile Modulus 55.0 MPa50mm/min; ISO 527-2/1A
Flexural Strength 4.00 MPaISO 178
 2.00 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 45.0 MPaISO 178
 26.0 MPa
@Temperature 100 °C
ISO 178
 270 MPa
@Temperature -40.0 °C
ISO 178
Resilience 58Bayshore, %
Flex Crack Resistance >= 1.00e+6Ross flex
Izod Impact, Notched (ISO) NBISO 180
 NB
@Temperature -30.0 °C
ISO 180/1U
 NB
@Temperature 23.0 °C
ISO 180/1U
 NB
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
Tear Strength 96.0 kN/mISO 34-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+12 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohmIEC 60093
Dielectric Constant 4.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 26.0 kV/mmIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 240 µm/m-°CISO 11359-2
Melting Point 195 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °CISO 75-1, -2
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 55.0 °Ccavity
 190 - 215 °Chot runner
Feed Temperature 185 - 200 °C
Zone 1 185 - 200 °C
Zone 2 185 - 210 °C
Zone 3 185 - 210 °C
Zone 4 185 - 215 °C
Die Temperature 190 - 215 °C
Melt Temperature 190 - 215 °C
Drying Temperature 100 - 110 °C
Dry Time 4.00 hour
Moisture Content <= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj\Blow\Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 2004-2 PBT, Unfilled
Celanese Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 655HS TPC, Unfilled
Celanese Riteflex® 447 TPC, Unfilled

PHCQ449 / 178904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.