MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zhejiang Juner PC-3-1 Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Applications: Shell of Small Household Electric Appliance

Information provided by Zhejiang Juner New Materials Co, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³GB/1033
Water Absorption 0.30 %0.30 %GB/T1034
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm0.0050 - 0.0060 in/inGB/15585
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 52.0 MPa7540 psiGB/1040
Flexural Strength 82.0 MPa11900 psiGB/9341
Charpy Impact Unnotched NBNBIS0179-1:2000
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²IS0179-1:2000
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmD257
Comparative Tracking Index 200 V200 VGB/4207
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FGB/1634
Flammability, UL94 HB - V-0HB - V-0GB/T2408
 
Processing PropertiesMetricEnglishComments
Processing Temperature 225 - 270 °C437 - 518 °F
Drying Temperature  100 °C
@Time 14400 sec
212 °F
@Time 4.00 hour
Chute Hot-Wind
 100 °C
@Time 18000 sec
212 °F
@Time 5.00 hour
Horizontal Oven
Injection Pressure 50.0 - 100 MPa7250 - 14500 psi
 
Descriptive Properties
Chromatism (?E)=0.8
Granule DiameterΦ3x3-5
Speed of Shoot, %35-80
Surface PolishHigh
WeatherabilityAdjustive

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJUNER47 / 48560

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.